General Frit GF-46

Description: Medium lead boron frit

Oxide Analysis Formula Tolerance
K2O 1.40% 0.04
Na2O 4.30% 0.21
CaO 7.30% 0.39
PbO 25.90% 0.35
Al2O3 2.20% 0.07
B2O3 16.30% 0.71
SiO2 42.60% 2.15
Oxide Weight 302.68
Formula Weight 302.68

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy