General Frit GF-146

Alternate Names: Frit 146, Frit GF146

Description: High sodium zinc borate frit (no silica)

Oxide Analysis Formula Tolerance
CaO 0.30% 0.02
K2O 1.00% 0.03
Na2O 16.40% 0.80
ZnO 4.20% 0.16
B2O3 54.20% 2.35
Al2O3 23.90% 0.71
Oxide Weight 301.14
Formula Weight 301.14

Notes

For use in low temperature 'faux-crystal' special-effect glazes and for bonding of abrasives.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 210R
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy