General Frit GF-106

Alternate Names: Frit 106, Frit GF106, GF 106, GC 106,Frit GF-106

Description: High-sodium high expansion frit

Oxide Analysis Formula Tolerance
CaO 0.33% 0.02
MgO 0.70% 0.06
Na2O 16.57% 0.92
Al2O3 5.93% 0.20
SiO2 76.47% 4.38
Oxide Weight 344.22
Formula Weight 344.22

Notes

Useful for cone 10 crystalline glazes.
Some sources claim that Hommel 529 is a substitute, but they are quite different.

Related Information

Links

Materials Pemco Frit P-278
Materials Hommel Frit 4GF152E
Materials Ferro Frit 3293
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit F-413
Materials Bayer Frit J-239-P
Materials Pemco Frit P-283
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.20
Frit Softening Point 1920F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy