Fusion Frit F-413

Alternate Names: Fusion Frit 413

Description: High sodium, boron-free, high expansion frit

Oxide Analysis Formula Tolerance
Na2O 17.00% 0.96
MgO 0.50% 0.04
Al2O3 5.50% 0.19
SiO2 76.50% 4.44
Oxide Weight 347.17
Formula Weight 347.17

Notes

Popular in crystalline glazes.

Related Information

Links

Materials Bayer Frit J-239-P
Materials General Frit GF-106
Materials Pemco Frit P-283
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.67 x 10e-6
Frit Softening Point 1600F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy