G20 HP Feldspar

Oxide Analysis Formula Tolerance
CaO 0.75% 0.08
K2O 13.20% 0.79
Na2O 1.52% 0.14
Al2O3 18.20% 1.00
SiO2 65.90% 6.16
Fe2O3 0.09% -
LOI 0.16%n/a
Oxide Weight 559.85
Formula Weight 560.75

Notes

Same chemistry as G200HP.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.