G&W Moss Clay

Description: Semi plastic, cream burning clay, high alkali content

Oxide Analysis Formula Tolerance
SiO2 58.50% 3.53
Al2O3 28.10% 1.00
Fe2O3 0.90% 0.02
TiO2 1.40% 0.06
MgO 0.10% 0.01
CaO 0.10% 0.01
Na2O 0.80% 0.05
K2O 2.80% 0.11
LOI 6.70%n/a
Oxide Weight 336.49
Formula Weight 360.65

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy