Fusion Frit FZ-84

Alternate Names: Frit FZ84

Description: Zinc alkaline frit

Oxide Analysis Formula Tolerance
CaO 5.10% 0.23
K2O 8.60% 0.24
MgO 0.60% 0.04
Na2O 4.50% 0.19
ZnO 9.60% 0.30
ZrO2 3.20% 0.07
B2O3 4.80% 0.18
Al2O3 13.40% 0.34
SiO2 50.30% 2.16
Oxide Weight 258.25
Formula Weight 258.25

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-1225
Materials Ferro Frit 3820
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy