Fusion Frit FZ-81

Description: Mystery frit without exact chemistry

Oxide Analysis Formula Tolerance
Li2O 2.50% 0.26 .5
Na2O 6.50% 0.32 2.5
K2O 2.50% 0.08 1.5
CaO 4.50% 0.24 1.5
ZnO 1.50% 0.06 1.5
SrO 1.50% 0.04 1.5
Al2O3 12.50% 0.37 2.5
B2O3 12.50% 0.55 2.5
SiO2 55.00% 2.79 5
Oxide Weight 301.47
Formula Weight 301.47

Notes

We only have ranges for the chemistry on this material.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.2
Frit Softening Point 1350C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy