1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit FZ-565

Alternate Names: Fusion Frit FZ565

Description: CaZn frit for slow fire

Oxide Analysis Formula Tolerance
Al2O3 8.50% 0.17
MgO 0.50% 0.03
ZnO 11.20% 0.28
CaO 13.50% 0.49
Na2O 5.80% 0.19
K2O 0.50% 0.01
B2O3 1.50% 0.04
SiO2 58.50% 1.99
Oxide Weight 204.29
Formula Weight 204.29

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.78 x 10-6
Frit Softening Point 1550F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy