1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit FZ-376A

Alternate Names: Fusion Frit FZ376A

Description: Fast fire Opaque Frit

Oxide Analysis Formula Tolerance
CaO 6.00% 0.48
K2O 2.80% 0.13
Na2O 4.60% 0.33
ZnO 1.10% 0.06
ZrO2 8.50% 0.31
B2O3 13.20% 0.85
Al2O3 7.60% 0.33
SiO2 56.20% 4.17
Oxide Weight 445.67
Formula Weight 445.67

Notes

This analysis was confirmed with Fusion Sept 2013.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-4K05
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Glossary Fast Fire Glazes
Industrial ceramics are fired very quickly and require minimal micro bubbles and zero pinholes and blisters. Fast fire late melting glazes accomplish that.

Data

Co-efficient of Linear Expansion 6.54
Frit Softening Point 1700F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy