Alternate Names: Fusion Frit F71
Description: Alkaline flux for grinding wheels
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 6.00% | 0.23 | |
| K2O | 2.50% | 0.06 | |
| Na2O | 20.40% | 0.71 | |
| B2O3 | 6.00% | 0.19 | |
| Al2O3 | 6.80% | 0.14 | |
| SiO2 | 58.30% | 2.10 | |
| Oxide Weight | 216.21 | ||
| Formula Weight | 216.21 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3281
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 11.31 x 10-6 |
|---|---|
| Frit Softening Point | 1400F |