Fusion Frit F-708

Oxide Analysis Formula Tolerance
K2O 6.00% 0.13
Na2O 27.00% 0.87
Al2O3 6.00% 0.12
B2O3 12.00% 0.35
SiO2 49.00% 1.63
Oxide Weight 200.33
Formula Weight 200.33

Notes

Chemistry is approximate.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.