1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-326

Alternate Names: Fusion Frit F326

Description: Opaque frit

Oxide Analysis Formula Tolerance
K2O 2.30% 0.10
Na2O 6.00% 0.41
CaO 4.50% 0.34
MgO 1.50% 0.16
Al2O3 8.60% 0.35
B2O3 10.60% 0.64
SiO2 56.50% 3.94
ZrO2 10.00% 0.34
Oxide Weight 419.07
Formula Weight 419.07

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.6 x 10-6
Frit Softening Point 1600F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy