Alternate Names: Fusion Frit F300
Description: Strontium frit for sanitaryware
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.00% | 0.56 | |
| K2O | 1.80% | 0.06 | |
| Na2O | 2.70% | 0.14 | |
| SrO | 8.20% | 0.25 | |
| B2O3 | 5.00% | 0.22 | |
| Al2O3 | 10.10% | 0.31 | |
| SiO2 | 62.40% | 3.24 | |
| Oxide Weight | 313.07 | ||
| Formula Weight | 313.07 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Pemco Frit P-4K47
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.29 |
|---|---|
| Frit Softening Point | 1800F |