Fusion Frit F-18

Alternate Names: F18 Fusion, Frit F18, Frit F 18

Description: Dinnerware Strontium Frit

Oxide Analysis Formula Tolerance
CaO 11.80% 0.59
K2O 2.40% 0.07
Na2O 2.60% 0.12
SrO 8.00% 0.22
B2O3 8.90% 0.36
Al2O3 6.80% 0.19
SiO2 59.50% 2.79
Oxide Weight 281.71
Formula Weight 281.71

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 630
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.13
Frit Softening Point 1750F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy