1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-13

Alternate Names: Frit F13

Description: Fast Fire Calcium Frit

Oxide Analysis Formula Tolerance
CaO 18.00% 0.70
K2O 0.15% -
Na2O 8.50% 0.30
B2O3 18.50% 0.58
Al2O3 4.50% 0.10
SiO2 50.35% 1.82
Oxide Weight 217.61
Formula Weight 217.61

Related Information

Links

Materials Pemco Frit P-926
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3288
Materials General Frit GF-103
Materials Ferro Frit 3814
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Glossary Fast Fire Glazes
Industrial ceramics are fired very quickly and require minimal micro bubbles and zero pinholes and blisters. Fast fire late melting glazes accomplish that.

Data

Co-efficient of Linear Expansion 8.03
Frit Softening Point 1525F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy