Frit VO 6257

Description: Reimbold & Strick fast double firing opaque frit

Oxide Analysis Formula Tolerance
K2O 6.00% 0.14
ZnO 13.00% 0.35
B2O3 10.00% 0.31
ZrO2 10.00% 0.18
CaO 10.00% 0.39
MgO 2.00% 0.11
SiO2 42.00% 1.52
PbO 2.00% 0.02
Al2O3 5.00% 0.11
Oxide Weight 217.28
Formula Weight 217.28

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 65 x 10-7 (20-400C)
Frit Softening Point 720C
Glass Transition Temperature 610C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy