Description: Leaded boron low-alumina frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 4.65% | 0.31 | |
| K2O | 1.70% | 0.07 | |
| Na2O | 1.69% | 0.10 | |
| PbO | 31.64% | 0.52 | |
| B2O3 | 13.02% | 0.69 | |
| Al2O3 | 3.17% | 0.12 | |
| SiO2 | 44.13% | 2.72 | |
| Oxide Weight | 370.39 | ||
| Formula Weight | 370.39 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3417
|
| Materials |
Ferro Frit 3493
|
| Materials |
Hommel Frit 24
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |