Frit A 3129

Description: Reimbold & Strick stoneware zinc matte frit

Oxide Analysis Formula Tolerance
PbO 45.00% 0.37
ZnO 25.00% 0.56
Al2O3 3.00% 0.05
CaO 1.00% 0.03
K2O 2.00% 0.04
SiO2 24.00% 0.73
Oxide Weight 182.55
Formula Weight 182.55

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 62 x 10-7 (20-400C)
Frit Softening Point 560C
Glass Transition Temperature 490C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy