Frit 1817

Description: High alkali leadless aluminun silicate frit

Oxide Analysis Formula Tolerance
CaO 13.96% 0.41
K2O 4.79% 0.08
MgO 0.86% 0.03
Na2O 18.10% 0.48
TiO2 0.04% -
Al2O3 8.46% 0.14
P2O5 0.03% -
SiO2 53.40% 1.45
Fe2O3 0.37% -
Oxide Weight 163.10
Formula Weight 163.10

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy