Frit 1047

Alternate Names: 1047 Boraksfritte

Description: Calcium borate frit

Oxide Analysis Formula Tolerance
CaO 10.79% 0.56
K2O 2.41% 0.07
Na2O 7.91% 0.37
Al2O3 17.85% 0.51
B2O3 20.41% 0.85
SiO2 40.63% 1.96
Oxide Weight 289.44
Formula Weight 289.44

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy