1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Richoux Frit 21 C002

Alternate Names: Frit 21 C002

Description: Fritte Boracique

Oxide Analysis Formula Tolerance
K2O 8.72% 0.21
Na2O 11.74% 0.43
CaO 8.57% 0.35
MgO 0.03% -
Al2O3 9.01% 0.20
B2O3 13.39% 0.44
SiO2 48.53% 1.85
Oxide Weight 229.63
Formula Weight 229.63

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 920-1050C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy