Ferro Frit CE VTR 29

Alternate Names: Frit VTR 29, Frit VTR29

Description: Lead bisilicate frit

Oxide Analysis Formula Tolerance
PbO 65.00% 1.00
SiO2 35.00% 2.00
Oxide Weight 343.38
Formula Weight 343.38

Notes

Their web page does not give the chemistry, but does indicate the presence of Al2O3 and KNaO. We assume these are in small amounts since they call this a lead bisilicate.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3498
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Ferro Frit 4064
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 980-1020C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy