Ferro Frit 4064

Alternate Names: Frit 4364, Frit 3531, Frit DA4064

Description: Lead alumina bilsilicate frit with small amount of sodium

Oxide Analysis Formula Tolerance
Na2O 0.97% 0.05
PbO 64.92% 0.95
Al2O3 2.02% 0.06
SiO2 32.10% 1.74
Oxide Weight 326.29
Formula Weight 326.29

Notes

Formerly Frit 4364

Related Information

Links

Materials Ferro Frit 3498
Materials Ferro Frit 4364
Materials Ferro Frit 3602
A lead bisilicate frit with 2.5% alumina oxide.
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit CE VTR 29
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.

Data

Frit Softening Point 510C
Density (Specific Gravity) 4.50
Frit Melting Range (C) 950-1080C
Glass Transition Temperature 465C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy