Ferro Frit CC-262

Alternate Names: Frit CC262

Oxide Analysis Formula Tolerance
BaO 2.40% 0.12
ZnO 9.20% 0.88
Oxide Weight 90.15
Formula Weight 90.15

Notes

One source specified SiO2:Al2O3 ratio of: 11.04
Alkalies: less than 5%
CaO: 5-10-%
MgO: less than 5%
Al2O3: 5-10%
SiO2: 5-10%
SiO2: More than 50%

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.2

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy