1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 4113

Alternate Names: Frit KFG 4113, Frit 4712, Frit DA4113

Description: General purpose hard and versatile borosilicate frit

Oxide Analysis Formula Tolerance
CaO 9.28% 0.59
Na2O 4.84% 0.28
B2O3 12.73% 0.65
SiO2 59.58% 3.53
K2O 3.53% 0.13
Al2O3 10.05% 0.35
Oxide Weight 355.96
Formula Weight 355.96

Notes

Formerly Frit 4712. Considered good for developing colors.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 4712
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 586C
Frit Melting Range (C) 1040-1100C
Glass Transition Temperature 652C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy