1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ferro Frit 4101

Alternate Names: Formerly Ferro Frit 530

Description: High expansion sodium borosilicate fluorine frit

Oxide Analysis Formula Tolerance
CaO 1.90% 0.08
K2O 20.35% 0.50
Na2O 11.05% 0.42
F 4.35% 0.53
Al2O3 7.22% 0.17
B2O3 11.18% 0.38
SiO2 43.95% 1.71
Oxide Weight 233.58
Formula Weight 233.58

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 530
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy