Description: Strontium fluxed all fritted leadless clear glaze
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 11.10% | 0.57 | |
| K2O | 3.40% | 0.10 | |
| Na2O | 1.70% | 0.08 | |
| SrO | 8.60% | 0.24 | |
| B2O3 | 8.80% | 0.37 | |
| Al2O3 | 6.20% | 0.18 | |
| SiO2 | 60.20% | 2.91 | |
| Oxide Weight | 290.37 | ||
| Formula Weight | 290.37 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 630
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.5 |
|---|---|
| Frit Melting Range (C) | 1750F |