Ferro Frit 3043

Description: Netherland, Flanders area (Ferro?)

Oxide Analysis Formula Tolerance
CaO 7.18% 0.43
B2O3 6.42% 0.31
SiO2 54.20% 3.03
Al2O3 6.07% 0.20
Na2O 2.03% 0.11
K2O 3.93% 0.14
MgO 0.24% 0.02
PbO 19.93% 0.30
Oxide Weight 335.91
Formula Weight 335.91

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy