1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Feldspar P. Tuerto (Cuba)

Description: Cuban feldspar

Oxide Analysis Formula Tolerance
SiO2 72.00% 7.36
Al2O3 15.40% 0.93
TiO2 0.01% -
CaO 1.40% 0.15
MgO 0.85% 0.13
K2O 4.30% 0.28
Na2O 4.40% 0.44
Fe2O3 0.27% 0.01
1.00% -
LOI 1.00%n/a
Oxide Weight 606.35
Formula Weight 612.47

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.