Eureka Feldspar

Description: Legacy low calcium potash feldspar

Oxide Analysis Formula Tolerance
CaO 0.01% -
K2O 9.37% 0.64
Na2O 3.49% 0.36
Al2O3 17.05% 1.07
SiO2 69.70% 7.44
Fe2O3 0.11% -
LOI 0.20%n/a
Oxide Weight 639.55
Formula Weight 640.83

Related Information

Links

Materials Custer Feldspar (pre-2000)
The most common potash feldspar used in ceramics in North America. It was a standard for many decades but is no longer available.
Materials Potash Feldspar
A feldspar having a KNaO content that predominates in potassium.
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy