1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Esmalte Frit PR-1000

Description: Esmalte Calcium borate frit

Oxide Analysis Formula Tolerance
MgO 0.80% 0.05
Na2O 2.20% 0.10
Al2O3 4.50% 0.12
SiO2 48.20% 2.20
B2O3 25.50% 1.01
Fe2O3 0.25% -
CaO 15.60% 0.76
K2O 2.90% 0.08
Oxide Weight 274.44
Formula Weight 274.44

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.