| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 5.20% | 0.12 | |
| CaO | 10.20% | 0.39 | |
| Al2O3 | 5.60% | 0.12 | |
| Fe2O3 | 0.10% | - | |
| ZrO2 | 7.60% | 0.13 | |
| Na2O | 0.50% | 0.02 | |
| ZnO | 10.70% | 0.28 | |
| SiO2 | 56.60% | 2.02 | |
| MgO | 3.60% | 0.19 | |
| Oxide Weight | 214.87 | ||
| Formula Weight | 214.87 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Frit Softening Point | 940C |
|---|---|
| Frit Melting Range (C) | 1170C |