Alternate Names: ESF501FG
Description: Turkish Soda Feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 70.00% | 6.66 | |
| Al2O3 | 18.00% | 1.01 | |
| Fe2O3 | 0.05% | - | |
| TiO2 | 0.05% | - | |
| CaO | 0.30% | 0.03 | |
| MgO | 0.20% | 0.03 | |
| K2O | 0.30% | 0.02 | |
| Na2O | 10.00% | 0.92 | |
| LOI | 0.30% | n/a | |
| Oxide Weight | 565.84 | ||
| Formula Weight | 567.54 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| Ultimate Particle Size Distribution | +200 3.50 +100 13.00 +74 24.50 +63 6.00 +45 13.00 -45 40.00 |
|---|