1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

English Kaolin

Description: White Burning High Flux Kaolin

Formula: Al2O3.SiO2

Oxide Analysis Formula Tolerance
CaO 0.02% -
K2O 1.79% 0.05
MgO 0.28% 0.02
Na2O 0.05% -
TiO2 0.06% -
Al2O3 37.38% 1.00
SiO2 47.44% 2.15
Fe2O3 0.82% 0.01
LOI 12.16%n/a
Oxide Weight 239.69
Formula Weight 272.87

Notes

There are a great many kaolins available from the UK. These are generally less plastic and fire to greater maturity than American counterparts (because they often contain significant K2O, MgO, etc). They are known for being cleaner and burning to a more blue-white color (whereas American materials more often burn to yellow-white).

Related Information

Links

Materials Standard Porcelain Kaolin
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Materials Treviscoe Kaolin
Materials Remblend Kaolin
Materials NSC Kaolin
Materials Super Standard Porcelain
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
Typecodes Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy