| Monthly Tech-Tip | No tracking! No ads! |
Alternate Names: Del Monte Feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.03 | |
| K2O | 4.30% | 0.35 | |
| MgO | 0.20% | 0.04 | |
| Na2O | 4.70% | 0.58 | |
| TiO2 | 0.02% | - | |
| Al2O3 | 16.50% | 1.24 | |
| SiO2 | 73.40% | 9.40 | |
| Fe2O3 | 0.15% | 0.01 | |
| LOI | 0.45% | n/a | |
| Oxide Weight | 765.26 | ||
| Formula Weight | 768.72 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| By Tony Hansen Follow me on ![]() | ![]() |