1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Degussa Frit 90321

Alternate Names: Zinkbarium fritte

Description: Zinkbarium-fritte

Oxide Analysis Formula Tolerance
ZnO 14.74% 0.40
BaO 27.77% 0.40
PbO 20.21% 0.20
Al2O3 4.62% 0.10
SiO2 32.66% 1.20
Oxide Weight 220.86
Formula Weight 220.86

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 99 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 507C
Heating Microscope Analysis for Frits 770C
Heating Microscope Analysis for Frits 980C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy