| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 25.10% | 0.90 | |
| K2O | 4.00% | 0.09 | |
| CaO | 0.10% | - | |
| Al2O3 | 11.80% | 0.26 | |
| SiO2 | 58.80% | 2.18 | |
| Oxide Weight | 222.23 | ||
| Formula Weight | 222.23 | ||
This frit is referenced in the book "Macro-Crystalline Glazes" by Peter Ilsley.
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |