Degussa Frit 90191

Alternate Names: 90191 Alkaliborfritte

Description: Alkaliborfritte

Oxide Analysis Formula Tolerance
CaO 1.12% 0.10
K2O 7.49% 0.40
SiO2 63.36% 5.30
B2O3 9.69% 0.70
Na2O 6.17% 0.50
Al2O3 12.17% 0.60
Oxide Weight 502.53
Formula Weight 502.53

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 76 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 543C
Heating Microscope Analysis for Frits 830C
Heating Microscope Analysis for Frits 1250C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy