Oxide Analysis Formula Tolerance
SiO2 56.35% 4.00
B2O3 16.31% 1.00
CaO 9.86% 0.75
K2O 5.52% 0.25
Al2O3 11.95% 0.50
Oxide Weight 426.66
Formula Weight 426.66

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 56 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 600C
Heating Microscope Analysis for Frits 865C
Heating Microscope Analysis for Frits 1050C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy