Degussa Frit 90167

Alternate Names: Alkaliborfritte

Description: High alkali borosilicate frit

Oxide Analysis Formula Tolerance
SiO2 43.93% 1.80
B2O3 16.96% 0.60
Al2O3 8.28% 0.20
CaO 2.28% 0.10
Na2O 11.33% 0.45
K2O 17.21% 0.45
Oxide Weight 246.23
Formula Weight 246.23

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 150 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 455C
Heating Microscope Analysis for Frits 646C
Heating Microscope Analysis for Frits 740C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy