Degussa Frit 90016

Alternate Names: 90016 Alkaliborfritte

Description: Alkaibortntte

Oxide Analysis Formula Tolerance
CaO 7.37% 0.50
B2O3 9.15% 0.50
Na2O 4.07% 0.25
K2O 6.19% 0.25
Al2O3 6.70% 0.25
SiO2 45.81% 2.90
Oxide Weight 301.79
Formula Weight 301.79

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 76 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 564C
Heating Microscope Analysis for Frits 790C
Heating Microscope Analysis for Frits 960C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy