Custer Feldspar (post-2000)

Alternate Names: Custer - low KnO

Oxide Analysis Formula Tolerance
SiO2 72.40% 8.63
Al2O3 15.27% 1.07
Fe2O3 0.21% 0.01
K2O 7.52% 0.57
Na2O 3.21% 0.37
CaO 0.27% 0.03
MgO 0.07% 0.01
P2O5 0.20% 0.01
LOI 0.65%n/a
Oxide Weight 710.43
Formula Weight 715.08

Notes

This is an average of actual assays done. See the notes for Custer Feldspar (pre-2000) for more info.

Related Information

Links

Materials Custer Feldspar (pre-2000)
The most common potash feldspar used in ceramics in North America. It was a standard for many decades but is no longer available.
URLs https://www.ronroy.net/analyses/custer-article-.pdf
Ron Roy article about changes in Custer Feldspar

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy