1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Challenger Ball Clay

Description: Low organics casting clay

Oxide Analysis Formula Tolerance
SiO2 54.10% 3.18
Al2O3 28.90% 1.00
Fe2O3 1.10% 0.02
TiO2 1.70% 0.08
CaO 0.20% 0.01
MgO 0.20% 0.02
K2O 0.30% 0.01
Na2O 0.20% 0.01
LOI 13.30%n/a
Oxide Weight 306.00
Formula Weight 352.94

Notes

This low organic premium blend combines very high plasticity and good casting rate using a proprietary dispersant system.
Legacy ball clay from K&T Clays

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.
Materials Challenger II Ball Clay

Data

% < 0.5 microns 46.0%
Drying Shrinkage 8.3%
Firing Shrinkage 9.5% at cone 9
Water absorption 9.0% at cone 9
Dry M.O.R. (50% Silica) 360 psi

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy