1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ceradel Frit C 1253

Alternate Names: Fritte C1253, Fritte C 1253, Ceradel Frit 1253

Description: High expansion frit, Fritte boro-alcaline sans plomb

Oxide Analysis Formula Tolerance
BaO 2.54% 0.05 10
B2O3 21.72% 0.95 10
Al2O3 6.43% 0.19 15
Na2O 13.37% 0.66 3
CaO 3.91% 0.21 .5
ZnO 2.16% 0.08
SiO2 49.86% 2.53
Oxide Weight 304.43
Formula Weight 304.43

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Co-efficient of Linear Expansion 99x10-7 (20/300C)
Frit Softening Point 880-920C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy