Ceradel Frit 3110

Alternate Names: Ceradel Fritte 3110

Description: High sodium, low boron/alumina frit

Oxide Analysis Formula Tolerance
CaO 6.50% 0.30
K2O 2.50% 0.07
Na2O 15.50% 0.64
B2O3 2.50% 0.09
Al2O3 4.00% 0.10
SiO2 69.00% 2.93
Oxide Weight 254.84
Formula Weight 254.84

Notes

Ceradel provides a slightly different chemistry for this than Ferro does for its 3110 standard formulation.

Related Information

Links

Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts at very low temperatures. Useful to make crackle glazes.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 100.8 (10-7/C 20/300C)
Frit Melting Range (C) 1000-1300C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy