BPS Standard Borax Frit

Description: Borax Frit

Oxide Analysis Formula Tolerance
CaO 14.22% 0.60
K2O 1.57% 0.04
MgO 0.17% 0.01
Na2O 9.02% 0.35
B2O3 17.94% 0.61
Al2O3 7.63% 0.18
SiO2 49.46% 1.96
Oxide Weight 238.23
Formula Weight 238.23

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials PotteryCrafts Frit P2953
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy