1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

BPS Calcium Borate Frit

Description: Calcium Borate Frit

Oxide Analysis Formula Tolerance
CaO 26.61% 0.98
K2O 0.45% 0.01
MgO 0.19% 0.01
B2O3 50.01% 1.49
Al2O3 4.89% 0.10
SiO2 17.85% 0.61
Oxide Weight 206.68
Formula Weight 206.68

Notes

Chemistry similar to colemanite

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron).
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy