Description: Cedar Heights Bonding
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.01 | |
| K2O | 1.70% | 0.06 | |
| MgO | 0.30% | 0.03 | |
| Na2O | 0.20% | 0.01 | |
| TiO2 | 1.60% | 0.07 | |
| Al2O3 | 29.40% | 1.00 | |
| SiO2 | 54.70% | 3.16 | |
| Fe2O3 | 1.70% | 0.04 | |
| LOI | 10.10% | n/a | |
| Oxide Weight | 311.55 | ||
| Formula Weight | 346.55 | ||
AVailable in 12/30/200 mesh sizes.
A light buff burning fireclay.

This picture has its own page with more detail, click here to see it.
They are fired from cone 4 to 10 oxidation (top down) and cone 10 reduction (bottom).
| Materials |
Goldart
|
| Materials |
Industrial Fireclay
|
| Materials |
CKR Clay
|
| Materials |
Fireclay A/S
|
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| Pyrometric Cone Equivalent | 31 |
|---|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk