Oxide Analysis Formula Tolerance
CaO 2.99% 0.35
K2O 0.39% 0.03
MgO 14.33% 2.32
Na2O 0.08% 0.01
TiO2 0.80% 0.07
Al2O3 15.66% 1.00
SiO2 53.68% 5.82
Fe2O3 0.54% 0.02
LOI 11.52%n/a
Oxide Weight 576.24